MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SCG Chemicals P704JM Homopolymer polypropylene resin
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: SCG PP P704JM is a homopolymer polypropylene resin that is well-suited to healthcare and pharmaceutical products. P704JM has good process ability, high clarity and is compliant to FDA and USP requirements.P704JM can be injection molded and sterilized by ethylene oxide.

Applications: Syringe barrel, Cylindrical test tubes, Contact Lens Mold Shell, Applications required high transparency.

Features: Easy processing. High transparency. High stiffness.

Information provided by SCG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.910 g/ccASTM D 1505
Linear Mold Shrinkage, Flow 0.015 in/in
@Thickness 2.00 mm
TPE Method
Linear Mold Shrinkage, Transverse 0.014 in/in
@Thickness 2.00 mm
TPE Method
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100ASTM D785
Tensile Strength, Yield 41.2 MPaCrosshead speed 50 mm/min; ASTM D638
Elongation at Break 600 %Crosshead speed 50 mm/min.; ASTM D638
Flexural Modulus 1470 MPaASTM D790
Izod Impact, Notched 34.0 J/m
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Melting Point 163 °CASTM D2117
Deflection Temperature at 0.46 MPa (66 psi) 115 °CASTM D648
Vicat Softening Point 155 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 20 %ASTM D1003
 
Descriptive Properties
AppearanceNatural Pellet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSCGC782 / 278039

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.