MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Chemlon® 220 G Nylon 6, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Availability: Asia Pacific; Europe; North America

Fillers/Reinforcement: Glass Fiber, 20% Filler by Weight

Features: Good Processability; Good Toughness; High Strength

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³ASTM D792
Water Absorption 1.2 %
@Time 86400 sec
1.2 %
@Time 24.0 hour
ASTM D570
Maximum Moisture Content 0.200.20
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 131 MPa19000 psiASTM D638
Elongation at Yield 3.5 %3.5 %ASTM D638
Flexural Yield Strength 193 MPa28000 psiASTM D790
Flexural Modulus 5.69 GPa825 ksiASTM D790
Izod Impact, Notched 0.908 J/cm1.70 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 204 °C400 °FUnannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 271 °C520 °F
Middle Barrel Temperature 266 °C510 °F
Front Barrel Temperature 249 °C480 °F
Nozzle Temperature 249 °C480 °F
Melt Temperature 216 °C420 °F
Mold Temperature 60.0 - 93.3 °C140 - 200 °F
Drying Temperature 79.4 °C175 °F
Injection Pressure 34.5 - 138 MPa5000 - 20000 psi
Screw Speed 60 - 120 rpm60 - 120 rpm
 
Descriptive Properties
AppearanceNatural Color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0488 / 236979

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.