MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Galden® SV55 PFPE Solvent
Categories: Fluid; Solvent

Material Notes: Galden® SV grades are specifically recommended for use as solvents.

Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of service temperature ranges, are available. Uses include heat transfer, electronic reliability testing, vapor phase soldering, solvents (especially SV grades), and acid spill mitigation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.65 g/cc
@Temperature 25.0 °C
Solubility of Water 0.0014 %
Solubility 14 ppmin water
Kinematic Viscosity 0.45 cSt
@Temperature 25.0 °C
Vapor Pressure 100 torr
@Temperature 9.00 °C
 228 torr
@Temperature 20.0 °C
 950 torr
@Temperature 60.0 °C
Surface Tension 10 dynes/cm
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 22.0 cal/g
@Temperature 55.0 °C
at boiling point
Boiling Point 55.0 °C
 
Descriptive Properties
Autoignition TemperatureNone
Fire Point (°C)None
Flash Point (°C)None
ODP0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Galden® LS230 PFPE VPS Fluid
Syensqo (Solvay Specialty Polymers) Galden® SV70 PFPE Solvent
Syensqo (Solvay Specialty Polymers) Galden® SV135 PFPE Solvent
Syensqo (Solvay Specialty Polymers) Galden® SV110 PFPE Solvent
Syensqo (Solvay Specialty Polymers) Galden® LS200 PFPE VPS Fluid

WAUSI510 / 149984

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.