MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

SABIC CYCOLOY™ FR Resin CS9610 Polycarbonate + ABS (PC+ABS) (Asia)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: CYCOLOY CS9610 Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend is an injection moldable low smoke, non chlorinated/brominated flame retardant grade. It has good mechanical and impact properties and has a UL94 V0@2.0mm and 5VB@2.0mm flame rating.

Features: Low Smoke and Toxicity,Flame Retardant,Non-Chlorinated,Non-Brominated,High Impact Resistance

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.20 g/cc1.20 g/ccASTM D792
Moisture Absorption 0.0400 %0.0400 %Injection Molding
Viscosity 12 cP
@Load 5.00 kg,
Temperature 260 °C
12 cP
@Load 11.0 lb,
Temperature 500 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0060 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 260 °C
15 g/10 min
@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psi50 mm/min; ISO 527
 62.0 MPa8990 psi50 mm/min; ASTM D638
Tensile Strength, Yield 62.0 MPa8990 psi50 mm/min; ISO 527
 64.0 MPa9280 psi50 mm/min; ASTM D638
Elongation at Break >= 45 %>= 45 %50 mm/min; ISO 527
 55 %55 %50 mm/min; ASTM D638
Elongation at Yield 4.8 %4.8 %50 mm/min; ISO 527
 5.0 %5.0 %50 mm/min; ASTM D638
Tensile Modulus 2.40 GPa348 ksi1 mm/min; ISO 527
 2.60 GPa377 ksi50 mm/min; ASTM D638
Flexural Strength 98.0 MPa14200 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 98.0 MPa14200 psiyield, 2 mm/min; ISO 178
Flexural Modulus 2.44 GPa354 ksi1.3 mm/min, 50 mm span; ASTM D790
 2.50 GPa363 ksi2 mm/min; ISO 178
Izod Impact Notched 800 J590 ft-lbASTM D256
Izod Impact, Notched (ISO) 45.0 kJ/m²21.4 ft-lb/in²80*10*3; ISO 180/1A
 15.0 kJ/m²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
80*10*3; ISO 180/1A
Charpy Impact, Notched 4.50 J/cm²21.4 ft-lb/in²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 1.50 J/cm²
@Temperature -30.0 °C
7.14 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 72.0 J53.1 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 118 °C
@Thickness 3.20 mm
244 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 106 °C223 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 105 °C
@Thickness 3.20 mm
221 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 124 °C255 °FRate B/50; ISO 306
 127 °C261 °FRate B/120; ISO 306
UL RTI, Electrical 90.0 °C194 °FUL 746B
UL RTI, Mechanical with Impact 90.0 °C194 °FUL 746B
UL RTI, Mechanical without Impact 90.0 °C194 °FUL 746B
Flammability, UL94  V-0
@Thickness >=2.00 mm
V-0
@Thickness >=0.0787 in
UL 94
 5VB
@Thickness >=2.00 mm
5VB
@Thickness >=0.0787 in
UL 94
Smoke Density 4040Flaming, Ds 1.5 min; ASTM E662
 150150Flaming, Ds 4 min; ASTM E662
 225225Flaming, Dmax; ASTM E662
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 265 - 300 °C509 - 572 °F
Zone 2 260 - 300 °C500 - 572 °F
Zone 3 265 - 300 °C509 - 572 °F
Melt Temperature 270 - 300 °C518 - 572 °FInjection Molding
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 90.0 °C194 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 80 %40 - 80 %
Vent Depth 0.00380 - 0.00760 cm0.00150 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm
Precipitation Temperature 60.0 - 80.0 °C140 - 176 °FHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH80017 / 287964

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.