Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.83 g/cc | 1.83 g/cc |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore A | 95 | 95 |
| 86 @Treatment Temp. 200 °C, Time 252000 sec | 86 @Treatment Temp. 392 °F, Time 70.0 hour |
| 89 @Treatment Temp. 200 °C, Time 252000 sec | 89 @Treatment Temp. 392 °F, Time 70.0 hour |
| 92 @Treatment Temp. 23.0 °C, Time 252000 sec | 92 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 92 @Treatment Temp. 100 °C, Time 252000 sec | 92 @Treatment Temp. 212 °F, Time 70.0 hour |
| 93 @Treatment Temp. 23.0 °C, Time 252000 sec | 93 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 93 @Treatment Temp. 150 °C, Time 252000 sec | 93 @Treatment Temp. 302 °F, Time 70.0 hour |
| 94 @Treatment Temp. 150 °C, Time 252000 sec | 94 @Treatment Temp. 302 °F, Time 70.0 hour |
| 95 @Treatment Temp. 23.0 °C, Time 252000 sec | 95 @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 95 @Treatment Temp. 250 °C, Time 252000 sec | 95 @Treatment Temp. 482 °F, Time 70.0 hour |
| 96 @Treatment Temp. 275 °C, Time 252000 sec | 96 @Treatment Temp. 527 °F, Time 70.0 hour |
Tensile Strength | 11.87 MPa | 1722 psi |
| 3.80 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 551 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 4.393 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 637.1 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 8.7625 MPa @Treatment Temp. 275 °C, Time 252000 sec | 1270.9 psi @Treatment Temp. 527 °F, Time 70.0 hour |
| 10.139 MPa @Treatment Temp. 200 °C, Time 252000 sec | 1470.6 psi @Treatment Temp. 392 °F, Time 70.0 hour |
| 10.258 MPa @Treatment Temp. 200 °C, Time 252000 sec | 1487.8 psi @Treatment Temp. 392 °F, Time 70.0 hour |
| 11.220 MPa @Treatment Temp. 150 °C, Time 252000 sec | 1627.3 psi @Treatment Temp. 302 °F, Time 70.0 hour |
| 11.909 MPa @Treatment Temp. 23.0 °C, Time 252000 sec | 1727.2 psi @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 11.980 MPa @Treatment Temp. 150 °C, Time 252000 sec | 1737.5 psi @Treatment Temp. 302 °F, Time 70.0 hour |
| 12.276 MPa @Treatment Temp. 250 °C, Time 252000 sec | 1780.5 psi @Treatment Temp. 482 °F, Time 70.0 hour |
Elongation, Ultimate | 130 % | 130 % |
| 29.9 % @Treatment Temp. 23.0 °C, Time 252000 sec | 29.9 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 101.7 % @Treatment Temp. 250 °C, Time 252000 sec | 101.7 % @Treatment Temp. 482 °F, Time 70.0 hour |
| 119.99 % @Treatment Temp. 200 °C, Time 252000 sec | 119.99 % @Treatment Temp. 392 °F, Time 70.0 hour |
| 130 % @Treatment Temp. 275 °C, Time 252000 sec | 130 % @Treatment Temp. 527 °F, Time 70.0 hour |
| 130 % @Treatment Temp. 23.0 °C, Time 252000 sec | 130 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 130 % @Treatment Temp. 23.0 °C, Time 252000 sec | 130 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 130 % @Treatment Temp. 150 °C, Time 252000 sec | 130 % @Treatment Temp. 302 °F, Time 70.0 hour |
| 130 % @Treatment Temp. 150 °C, Time 252000 sec | 130 % @Treatment Temp. 302 °F, Time 70.0 hour |
| 130 % @Treatment Temp. 200 °C, Time 252000 sec | 130 % @Treatment Temp. 392 °F, Time 70.0 hour |
100% Modulus | 9.777 MPa | 1418 psi |
Tear Strength | 27.9 kN/m | 159 pli |
| 35.1 kN/m | 200 pli |
Compression Set | 18.1 % @Treatment Temp. 175 °C, Time 79200 sec | 18.1 % @Treatment Temp. 347 °F, Time 22.0 hour |
| 22 % @Treatment Temp. 200 °C, Time 79200 sec | 22 % @Treatment Temp. 392 °F, Time 22.0 hour |
| 22.3 % @Treatment Temp. 23.0 °C, Time 79200 sec | 22.3 % @Treatment Temp. 73.4 °F, Time 22.0 hour |
|
Thermal Properties | Metric | English | Comments |
---|
Brittleness Temperature | -12.2 °C | 10.0 °F |
Shrinkage | 0.10 % @Treatment Temp. 23.0 °C, Time 252000 sec | 0.10 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 0.20 % @Treatment Temp. 150 °C, Time 252000 sec | 0.20 % @Treatment Temp. 302 °F, Time 70.0 hour |
| 1.0 % @Treatment Temp. 23.0 °C, Time 252000 sec | 1.0 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 1.3 % @Treatment Temp. 150 °C, Time 252000 sec | 1.3 % @Treatment Temp. 302 °F, Time 70.0 hour |
| 2.1 % @Treatment Temp. 23.0 °C, Time 252000 sec | 2.1 % @Treatment Temp. 73.4 °F, Time 70.0 hour |
| 2.2 % @Treatment Temp. 100 °C, Time 252000 sec | 2.2 % @Treatment Temp. 212 °F, Time 70.0 hour |
| 6.9 % @Treatment Temp. 200 °C, Time 252000 sec | 6.9 % @Treatment Temp. 392 °F, Time 70.0 hour |
| 11.2 % @Treatment Temp. 200 °C, Time 252000 sec | 11.2 % @Treatment Temp. 392 °F, Time 70.0 hour |
|
Descriptive Properties |
---|
Color | Black |
TR-10 Temperature | -19°C |