MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Westlake Plastics

(Viewing data as-entered. Click here to return)
Westlake Plastics Thermalux® PESU
Categories: Polymer; Thermoplastic; Polyethersulfone (PES)

Material Notes: Thermalux Polyethersulfone (PESU) Is an amber colored, semi-transparent, high performance engineering thermoplastic that combines good chemical resistance with a high heat deflection temperature (204°C / 399°F), making it a good fit for food service applications. This resin is also inherently flame retardant for use in electronic components and testing devices.

Applications include:

  • Electrical Connectors/Fittings
  • Burn in Test Sockets
  • Food Service Warming Trays
  • Safety face shields

Information provided by Westlake Plastics Co.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.24 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 10200 psiASTM D638
Elongation at Break 50 - 60 %ASTM D638
Elongation at Yield 5.0 - 6.0 %ASTM D638
Tensile Modulus 360000 psiASTM D638
Flexural Strength 15400 psiASTM D790
Flexural Yield Strength 15400 psiASTM D790
Flexural Modulus 390000 psiASTM D790
Compressive Yield Strength 13900 psiASTM D695
Izod Impact, Notched 1.30 ft-lb/inASTM D256
Izod Impact, Unnotched NBASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+16 ohm-cmASTM D257
Dielectric Constant 3.06
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 425 V/milASTM D149
Dissipation Factor 0.0010
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 31.0 µin/in-°FASTM D696
Thermal Conductivity 0.259 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 358 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 345 °FASTM D648
Flammability, UL94 V-0
@Thickness 4.47 mm
Oxygen Index 30 %ASTM D2863
 
Optical PropertiesOriginal ValueComments
Haze 5.0 %ASTM D1746
Transmission, Visible 75 %ASTM D1746
 
Descriptive Properties
ColorNatural (Transparent Amber)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWEST928 / 243172

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.