MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives Chemlok® 6227 Adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: LORD Chemlok® 6227 adhesive is a heat-activated adhesive which will bond a variety of elastomers to metal and plastic substrates during vulcanization of the elastomer. It is formulated without heavy metals and composed of a mixture of polymers and heat-reactive components in an organic solvent system. In some circumstances, Chemlok 6227 adhesive may be used as a single coat adhesive. For general use, it should be used in combination with an appropriate metal primer such as Chemosil® 211 primer. When used with Chemosil 211 primer, the environmental resistance of the final bond will be enhanced.

Features: bonds compounds based on natural rubber (NR), polyisoprene (IR), styrene-butadiene (SBR), polybutadiene (BR), polychloroprene (CR), nitrile (NBR), and butyl (IIR) elastomers to most metals, alloys and polar polymeric substrates. applies easily by spray, dip, brush or roll coat methods. accommodates a wide range of processing conditions, including extended prebake and elevated vulcanization temperatures. provides superior resistance to heat and salt spray.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.971 - 1.02 g/cc
@Temperature 20.0 °C
0.0351 - 0.0368 lb/in³
@Temperature 68.0 °F
Solids Content 22 - 26 %
@Temperature 130 °C,
Time 1800 sec
22 - 26 %
@Temperature 266 °F,
Time 0.500 hour
by weight, Dry residue
Brookfield Viscosity 100 - 400 cP
@Temperature 25.0 °C
100 - 400 cP
@Temperature 77.0 °F
Brookfield LVT, Spindle 2, 30 rpm
 
Thermal PropertiesMetricEnglishComments
Flash Point 29.0 °C84.2 °FSeta
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature 21.0 - 27.0 °C
12.0 Month
@Temperature 69.8 - 80.6 °F
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceBlack liquid
SolventsXylene

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLORD9007 / 232396

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.