MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
LyondellBasell Hyperzone HY4008 HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Hyperzone HY4008 is a bimodal, high molecular weight, high density polyethylene resin with excellent processing characteristics produced with LyondellBasell's new proprietary Hyperzone PE process technology. HY4008 is selected by customers for pressure pipe applications including gas distribution, industrial piping, mining, oil & gas gathering, municipal water lines and sewers. Customers typically use HY4008 in applications requiring an excellent balance of processability and toughness, along with high resistance to pipe failure by rapid crack propagation and slow crack growth mechanisms. When HY4008 is combined with a LyondellBasell approved color or black masterbatch at the correct use level, this compound may meet the following standards or requirements:
ASTM D2513-18a for Polyethylene (PE) Gas Pressure Pipe, Tubing and Fitting, Category C per Table 5
ASTM D3350 Cell Classifications: PE445574C and PE445576C.
CSA B137.1 for Pipe, Tubing and Fittings for Cold-Water Pressure Services
CSA B137.4 for Polyethylene Piping Systems for Gas Services: PE4710 PLUS & PE 100
NSF Standard 14 and Standard 61 for Potable Water Pipe and Fittings
NSF Standard 14 for Gas Distribution Applications
NSF Standard 358-1 for PE Pipe and Fittings for "Geothermal" Heat Pump Systems
Plastics Pipe Institute (PPI) PE4710 and PE 100 per PPI TR-3

Status: Commercial

Availability: Asia-Pacific; North America; South & Central America

Application: Drainage Pipe; Drinking Water Pipe; Gas Pipe; Industrial; Soil & Waste Pipe

Market: Industrial, Building & Construction; Pipe

Processing Method: Pipe

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9495 g/ccASTM D1505
Oxidative Induction Time (OIT) 140 min
@Temperature 200 °C
ASTM D3895
Melt Flow 0.280 g/10 min
@Load 5.00 kg,
Temperature 190 °C
ASTM D1238
 7.50 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
PENT >= 10000 hour
@Pressure 2.40 MPa,
Temperature 80.0 °C
on Black Compound, Air; ASTM F1473
 >= 10000 hour
@Pressure 2.40 MPa,
Temperature 80.0 °C
on Natural Resin, Air; ASTM F1473
Tensile Strength at Break 37.2 MPaASTM D638
Tensile Strength, Yield 25.6 MPaASTM D638
Elongation at Break 570 %ASTM D638
Flexural Modulus 1000 MPa2% Secant; ASTM D790
Hydrostatic Design Basis 1000 psi
@Temperature 60.0 °C
ASTM D2837
 1600 psi
@Temperature 22.8 °C
ASTM D2837
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -76.0 °CF50; ASTM D746
DSC Induction Temperature 260 °CASTM D3350
 
Descriptive Properties
Creep Rupture Strength>500 hr20 °C, 12.4 MPa, ISO 1167-1, -2
Minimum Required Strength10 MPaISO 12162
Notched Pipe Test>500 hr80°C, 0.92 MPa, ISO 13479
Resistance to Rapid Crack Propagation<-21 °CTc @ 5 bar (4"), ISO 13477
 <-9 °CTc @ 5 bar (12"), ISO 13477
 >12 barPc @ 32 °F, ISO 13477

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEQS9630 / 324565

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.