MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Cadmium Copper, UNS C16200, OSO25 Temper rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Good to excellent corrosion resistance. Excellent cold workability; good hot formability.

Applications: trolley wire, heating pads, electric-blanket elements, spring contacts, railbands, high-strength transmission lines, connectors, cable wrap, switch gear components and wave guide cavities.

Test specimen: rod - 13mm diameter; OS025 anneal (0.025 mm grain size).

Key Words: C108, ISO CuCd1, A1/3, cadmium bronze, copper-cadmium
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.89 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell F 46
Tensile Strength, Ultimate 250 MPa
Tensile Strength, Yield 83.0 MPa
Elongation at Break 57 %In 50 mm
Modulus of Elasticity 115 GPa
Poissons Ratio 0.307
Machinability 20 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 44.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000192 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 17.0 µm/m-°C
@Temperature 20.0 - 100 °C
 17.3 µm/m-°C
@Temperature 20.0 - 200 °C
 17.7 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 360 W/m-K
Melting Point 1030 - 1076 °C
Solidus 1030 °C
Liquidus 1076 °C
Annealing Point 800 - 1400 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 425 - 750 °C
Hot-Working Temperature 750 - 875 °C
 
Component Elements PropertiesOriginal ValueComments
Cadmium, Cd 0.70 - 1.2 %
Copper, Cu 98.78 - 99.3 %
Iron, Fe <= 0.020 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® SP-1 Polyimide, Machined
Commercial Bronze, UNS C22000 (90-10 Bronze), OSO25 Temper tubing
Commercial Bronze, UNS C22000 (90-10 Bronze), OSO35 Temper rod
Copper, UNS C62300 (Aluminum Bronze 9%), H50 Temper, 25 mm rod
Commercial Bronze, UNS C22000 (90-10 Bronze), H80 Temper tubing

MC16200b7 / 10711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.