MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

McDanel Advanced Ceramics AP 35 99% Alumina
Categories: Ceramic; Oxide; Aluminum Oxide

Material Notes: Information provided by McDanel Advanced Ceramic Technologies

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 3.83 g/cc0.138 lb/in³
Porosity 0.00 %0.00 %
 
Mechanical PropertiesMetricEnglishComments
Flexural Strength 345 MPa50000 psi
 205 MPa
@Temperature 538 °C
29700 psi
@Temperature 1000 °F
Compressive Strength 2550 MPa370000 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.40 µm/m-°C
@Temperature 20.0 - 1000 °C
4.67 µin/in-°F
@Temperature 68.0 - 1830 °F
Thermal Conductivity 29.0 W/m-K201 BTU-in/hr-ft²-°F
 7.20 W/m-K
@Temperature 800 °C
50.0 BTU-in/hr-ft²-°F
@Temperature 1470 °F
Maximum Service Temperature, Air 1750 °C3180 °Fno load
 
Component Elements PropertiesMetricEnglishComments
Al2O3 99 %99 %
CaO 0.030 %0.030 %
Fe2O3 0.070 %0.070 %
MgO 0.070 %0.070 %
Na2O 0.050 %0.050 %
SiO2 0.70 %0.70 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
MarkeTech Aluminum Oxide Ceramic - Alumina 99.5%
Alumina, alpha Al2O3, 99.5%
Alumina, alpha Al2O3, 96%
MarkeTech AN 180 Aluminum Nitride Ceramic Substrate, 99% Purity
MarkeTech AN 160 Aluminum Nitride Ceramic Substrate, 99% Purity

CMCDAN1 / 1497

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.