MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Quantum Composites QC-8777 41% Glass Fiber Reinforced Polyester Hybrid SMC
Categories: Polymer; Thermoset; Composite SMC; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: QC-8777 is a polyester hybrid engineered structural composite molding compound designed for compression molding of components requiring high structural strength, corrosion resistance and temperature resistance combined with low molded density.

  • Form = Rolls, Festooned Sheet
  • Color = Black, Natural
  • Glass Fiber Content = 41% nominal

A. Schulman has acquired Quantum Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/ccASTM D792
Water Absorption 0.13 %ASTM D570
 1.2 %
@Temperature 50.0 °C,
Time 3.60e+6 sec
ASTM D570
Linear Mold Shrinkage -0.00100 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 105 MPaASTM D638
Flexural Strength 235 MPaASTM D790
Flexural Modulus 11.4 GPaASTM D790
Izod Impact, Notched 960 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air >= 250 °CDeflection Temperature, Load not specified; ASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 320 °F
@Thickness 12.7 mm
Compression Molding
Clamp Pressure 300 - 1000 psi
Cure Time 3.00 - 5.00 min
@Thickness 6.35 mm,
Temperature 149 °C
Shelf Life 1.00 Month
@Temperature 23.9 °C
 
Descriptive Properties
Fiber Length (in)1Glass, nominal
FlammabilitySelf ExtinguishingFMVSS 302-75

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Quantum Composites QC-7753 50% Glass Fiber Reinforced Polyester SMC
Quantum Composites QC-8700 63% Glass Fiber Reinforced Vinyl Ester SMC
Applied Composites 120 Polyester SMC
A. Schulman Premi-Glas® 2204-30 CR-SX Fiberglass Reinforced SMC
Haysite 44500 Vinyl Ester SMC, 30% Glass Reinforced

PCOQB903 / 139271

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.