MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

LG Chemical HP-IPA ISOPROPYL ALCOHOL  (discontinued **)
Categories: Fluid

Material Notes: Features: IPA is produced by the direct propylene hydration process. IPA meets the diverse needs from solvent industry. Our division has been a stable supplier of raw materials for related industries. HP-IPA is used for cleaning semiconductor wafer and LCDs. This highly value-added product has been enjoying rapid increase in demand in accordance with the development of such areas as information, communication and multimedia. Low Water Content - IPA is highly hydrophilic product. so, water content control is very important. We manufacture IPA with a significantly low level of water content by strict maintenance of storage sealing and quality control. High Purity - We have high performance purification process to manufacture high purity IPA products. Our IPA maintains superior quality characteristics through products of high purity.

CAS No. 67-63-0

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.786 g/cc0.786 g/ccASTM D1298
Viscosity 2.2 cP
@Temperature 20.0 °C
2.2 cP
@Temperature 68.0 °F
Molecular Weight 60.01 g/mol60.01 g/mol
Vapor Pressure 0.00587 bar
@Temperature 20.0 °C
4.40 torr
@Temperature 68.0 °F
Vapor density: 2.1
 
Thermal PropertiesMetricEnglishComments
Flash Point 11.7 °C53.1 °F
Ignition Temperature 456 °C853 °FAutoignition
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.010 %<= 0.010 %ASTM D1364
 
Descriptive Properties
Acidity<10 ppmASTM D1613
Color5 APHAASTM D1209
Flammable limits in air2-12% (LEL)
Purity>99.99%Gas Chro.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLAY355 / 148365

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.