MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Solvay JAGUAR® HP 8 COS Surfactant
Categories: Fluid

Material Notes: Description: Hydroxypropyl Guar for thickening, which provides a fluid and smooth wet feel to formulations

Chemical Name: Guar Gum Derivative

C.T.F.A./I.N.C.I. Name: Hydroxypropyl Guar

CAS: 39421-75-5

Solubility: Soluble in water at 20°C. Insoluble in non-polar solvent

Available in: Asia Pacific, Europe, Latin America and North America

Applications: JAGUAR HP-8 COS is a nonionic naturally occurring polymer. Optimum thickening effect. Compatible with dilute-alcohol solutions containing up to 30% ethanol. Good compatibility with electrolytes and stability over a large range of pH. Smooth skin feel. Helps stabilize emulsions.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 g/cc0.0253 lb/in³
Particle Size >= 90 µm>= 90 µm150 Mesh; RP-0887
pH 8.5 - 118.5 - 11Inherent 1%; RP-0889
Viscosity 3600 - 4600 cP
@Time 7200 sec
3600 - 4600 cP
@Time 2.00 hour
RP-0891
 
Processing PropertiesMetricEnglishComments
Shelf Life 24.0 Month24.0 Month
 
Component Elements PropertiesMetricEnglishComments
H2O, Water 6.0 - 12 %6.0 - 12 %RP-0838
 
Descriptive Properties
AppearanceFine, creamy to pale yellow powder
CompositionGram Negative BacteriaNegative, RP-1445
 Mold<100 cfu/g, RP-1445
 Plate Count<1000 cfu/g, RP-1410
 Staphylococcus AureusNegative, RP-1445
 Yeast<100 cfu/g, RP-1445
Substitution level0.4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WRHOD179 / 137410

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.