MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SunChemical Gwent C2041206D2 Gold Polymer Electrode Paste  (discontinued **)
Categories: Fluid; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Gold Paste C2041206D2 is a screen printable gold polymer paste designed as a working electrode in electrochemical Biosensors. This paste is used as a working electrode in Medical Diagnostics, Environmental Sensor and the "Agri-Food" Industries, in conjunction with counter and reference electrodes.

The ink is in a ready to use form at a viscosity suitable for automatic or semiautomatic screen printing. The ink should be gently stirred before use avoiding introduction of air bubbles. It is a Polymer System for printing on polyester, PVC, Polycarbonate etc and on alumina.

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 81 - 82 %
 85 %
Particle Size 3.0 µmMain Break; Fineness of Grind
 10 µm3rd Streak; Fineness of Grind
Viscosity 12000 - 18000 cP
 20000 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
Haake VT550 cone and plate viscometer (PK1.1°)
Thickness 27.0 micronswhen printed through a 230 mesh SS screen
Storage Temperature 20.0 °C
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 110 ohmcured film; 27 microns thick
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °C
Cure Time 1 hour
Shelf Life 3.00 Month
 
Descriptive Properties
Conductive Filler TypeGold
Coverage cm2/g90230 mesh stainless steel screen
Material TypeReady-To-Use Formulation
Printing Mesh counts/inch120 to 200typical screen size is 156 Polyester
Solvent SystemEthoxy Propanol or Sericol

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SunChemical Gwent C2041206P2 Gold Polymer Electrode Paste

WGEM062 / 75915

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.