MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Saint-Gobain CHR® 2265-5 Extruded PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape; Thermoset; Silicone

Material Notes: CHR® 2265 is manufactured from high-modulus, extruded PTFE film coated with high-temperature silicone adhesive.

Features/Benefits: CHR® 2265 is an extruded, high-modulus PTFE tape utilizing a high temperature clean release silicone adhesive. 2265 has excellent chemical resistance and lies flat. The PTFE backing also provides an anti-friction and an easy release surface.

Applications: The excellent conformability and release properties of the PTFE backing, along with the high-temperature capabilities of the CHR® 2265, make the tape ideal for applications such as composite lay-up, roller wrapping, plate masking and other uses where costly clean up is a problem.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 250 %250 %
Tear Strength 11.4 kN/m65.0 pliInitial Tear Strength
Peel Strength 0.490 kN/m2.80 pliAdhesion to Steel
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 84.3 kV/mm2140 kV/in
Dielectric Breakdown 15000 V15000 V
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Descriptive Properties
ColorGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSTGQZ362 / 68876

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.