MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

RESPOL EBANTIX® E1303 EBA
Categories: Polymer; Thermoplastic; Ethylene Butyl Acrylate

Material Notes: Product Description: EBA REPSOL EBANTIX® E1303 is a copolymer suitable for blown film applications where good flexibility and very good mechanical properties are required. The butyl acrylate content is 13%. It contains antioxidant additives.
Applications: Film extrusion; Stretch hood film; Agricultural films; Cables
Recommended melt temperature 180°C. Processing characteristics of E1303 are similar to LDPE and conventional polyethylene extruders are recommended. Processing conditions should be optimized for each production line.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Antioxidant

Features: Antioxidant; Copolymer, Food Contact Acceptable; Good Flexibility

Uses: Agricultural Applications; Blow Molding Applications; Film; Stretch Wrap

Agency Ratings: EU Food Contact

Processing Method: Blown Film; Film Extrusion

Information provided by REPSOL

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.925 g/cc0.0334 lb/in³ISO 1183
Butyl Acrylate Content 13 %13 %
Melt Flow 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 570 %
@Thickness 0.203 mm
570 %
@Thickness 0.00800 in
Blown Film; ISO 527-3
Film Elongation at Break, TD 600 %
@Thickness 0.203 mm
600 %
@Thickness 0.00800 in
Blown Film; ISO 527-3
Coefficient of Friction 1.31.3ISO 8295
Elmendorf Tear Strength MD 1270 g
@Thickness 0.203 mm
1270 g
@Thickness 0.00800 in
Blown Film; ISO 6383-2
Elmendorf Tear Strength TD 1360 g
@Thickness 0.203 mm
1360 g
@Thickness 0.00800 in
Blown Film; ISO 6383-2
Dart Drop Test >= 1500 g
@Thickness 0.203 mm
>= 3.31 lb
@Thickness 0.00800 in
Blown Film; ISO 7765-1
Film Tensile Strength at Break, MD 20.0 MPa
@Thickness 0.203 mm
2900 psi
@Thickness 0.00800 in
Blown Film; ISO 527-3
Film Tensile Strength at Break, TD 22.0 MPa
@Thickness 0.203 mm
3190 psi
@Thickness 0.00800 in
Blown Film; ISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 101 °C214 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 °C356 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRESPOL1306 / 311999

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.