MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

ExxonMobil Vistalon™ 7001 Metallocene EPDM
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Vistalon 7001 EPDM rubber is a tailored MWD, high ethylene and medium diene polymer produced using ExxonMobil Chemical's EXXPOL™ Technology for precise control of molecular composition and architecture. It is applicable formolded and mechanical goods, hoses and extruded profiles. This product is sold in pellet form.

Key Features:

  • Designed for good physical properties, improved mixing, mill handling and extrusion compared to typical narrow MWD grades.
Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Mooney Viscosity 60
@Temperature 125 °C
60
@Temperature 257 °F
ML 1 + 4; ASTM D1646
 
Descriptive Properties
ENB Content5%ASTM D6047
Ethylene Content73%ASTM D3900

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Nordel® IP 4570 EPDM Hydrocarbon Rubber
ExxonMobil Vistalon™ 1703P EPDM
Dow Nordel® IP 4570 Radiator/Heater Hose
Avient Elastamax™ XL 0162-21 EPDM TPV-Based Thermoplastic Elastomer
Dow Nordel® IP 4570 Dense Extruded Profile

PEXB330 / 37635

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.