MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Nanocyl SIZICYL™ XC R2G Liquid Sizing Agent for Carbon and Glass Fibers
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: SIZICYL™ XC R2G is a liquid sizing agent containing Carbon Nanotubes for reinforcement fibers for composite applications. Specifically engineered to improve mechanical properties of the final composite structure, without affecting the viscosity of the resin used to impregnate the fiber (e.g. by resin infusion or RTM process), this formulation is designed according to industrial processings in order to bring an efficient answer to performance requirements in composite applications. SIZICYL™ XC R2G is compatible especially with glass and carbon fibers.

Applications: High performance composite parts

  • Automotive (bumpers and other structural parts)
  • Marine, especially sailing boats (structural outer shell in carbon fiber composite, masts and other generic structural parts)
  • Industrial parts (rollers, doctor-blades and wind-mill blades)
  • Sporting equipments (bike frames, hockey sticks, tennis rackets, skis and golf shafts)
  • Aerospace (structural parts and interiors)

Advantages Versatile application, Easy and ready to use, Compatible with RTM and Infusion processes

Suggested conditions of application SIZICYL™ XC R2G solid content is 6.2%. The suggested solid content on the surface of the fibers or the textile is 0.5%. Liquor pickup of SIZICYL™ XC R2G has to be adjusted accordingly to process setup (full bath impregnation or Roller impregnation for the fibers) to achieve the suggested solid content.

To comply with viscosity and process requirements, SIZICYL™ XC R2G can be diluted with de ionized water. Drying of SIZICYL™ XC R2G has to e done in the range of temperature between 150 and 175 degrees Celsius. SIZICYL™ XC R2G can be applied as a first layer of sizing agent or as an oversizing on the fibers or textiles. SIZICYL™ XC R2G is compatible with Carbon and glass fibers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EBS ACRALOCK SA10-07WHT Structural Methacrylate Adhesive
Nanocyl PREGCYL™ NC R2HM-01 Pre-impregnated UD/Fabric Carbon Fibers
DIAB Divinycell® P 60 Sandwich Core Material
DIAB Divinycell® P 150 Sandwich Core Material
DIAB Divinycell® P 120 Sandwich Core Material

ENANOC960 / 108955

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.