MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC SABIC® LLDPE M500026 PE (Global)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: M500026 is a Linear Low Density Polyethylene grade with narrow molecular weight distribution suitable for injection molding applications. It has been designed to give excellent flow properties with better low temperature toughness, stress crack resistance and gloss.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.926 g/cc0.0335 lb/in³ASTM D1505
Environmental Stress Crack Resistance 2.0 hour2.0 hourASTM D1693
ESCR 100% Igepal® 2.0 hour2.0 hourCO-630, F50; ASTM D1693B
Melt Flow 50 g/10 min
@Load 2.16 kg,
Temperature 190 °C
50 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5555ISO 868
Tensile Strength at Break 12.4 MPa1800 psiASTM D638
Tensile Strength, Yield 13.0 MPa1890 psiASTM D638
Elongation at Break 120 %120 %ASTM D638
1% Secant Modulus 354 MPa51300 psiASTM D638
Izod Impact, Notched 4.50 J/cm8.43 ft-lb/inASTM D256A
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 88.0 °C190 °Fat 10 N (VST/A); ASTM D1525
Brittleness Temperature <= -75.0 °C<= -103 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI11094 / 244561

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.