MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Grolltex Large Area CVD Graphene Film on Si/SiO2, 8" (200mm) Diameter
Categories: Carbon

Material Notes: Highest quality single layer graphene attainable. Chemical vapor deposition (CVD) produces the highest quality continuous monolayer graphene commercially available; as synthesized on copper and transferred to Si/SiO2, processed and packaged in an atmosphere free environment, shipped in double vacuum wrapped bags

Information provided by Grolltex, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.0 - 30 ohm-cmWafer
Surface Resistivity per Square 380 - 480 ohmGraphene Sheet
 
Optical PropertiesOriginal ValueComments
Transmission, Visible >= 97 %
 
Descriptive Properties
Graphene Coverage>95% with sporadic adlayers
Graphene FET Mobility>2700 cm2/(V.s)
Graphene Grain Size>30 microns
Graphene Raman D/G RatioIndistinguishable to 0.03
Wafer DopingP/B
Wafer Growth MethodCZ
Wafer Metal Impurities1.00e 10 - 5.00e 10 (at/cm2)
Wafer Oxide Thickness300nm
Wafer Si Orientation1-0-0
Wafer Thickness725 +/-25 microns

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow CVD Graphene Film on Copper Foil
Goodfellow CVD Graphene Film on Quartz Glass
Goodfellow Ultra Clean CVD Graphene Film on SiO2/Si Wafers
Grolltex Large Area CVD Graphene Film on Si/SiO2, 6" (150mm) Diameter
Goodfellow Reduced Graphene Oxide (GO) Powder

CGROL993 / 210151

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.