System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Beologic Beograde BTL035 Bottling
Categories:
Polymer
;
Thermoplastic
Material Notes:
Main properties: soft, glossy, good mechanical properties. Applications: blow molding extrusion, industrial and consumer goods, household, food packaging
Information provided by Beologic.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.15
-
1.25
g/cc
0.0415
-
0.0452
lb/in³
ISO 1183-1
Melt Flow
4.0
-
5.0
g/10 min
@Load 2.16 kg,
Temperature 190 °C
4.0
-
5.0
g/10 min
@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties
Metric
English
Comments
Tensile Strength
22.8
MPa
3310
psi
ISO 527
Elongation at Break
175 %
175 %
ISO 527
Tensile Modulus
1.34
GPa
194
ksi
ISO 527
Flexural Modulus
1.072
GPa
155.5
ksi
ISO 178
Charpy Impact, Notched
9.64
J/cm²
45.9
ft-lb/in²
ISO 179-1
Descriptive Properties
Beologic Article Number
9802070035
Biodegradable
yes
EN13432
Food contact approval
yes
Renewable content
yes
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PBEOL9885 / 314171
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.