MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

USI Corporation FREVA™ SES60 Stainless Steel Fiber Reinforced Composited Sheet
Categories: Other Engineering Material

Material Notes: Description:
  • FREVATM SES60 is a highly fire retardant material with excellent flexibility and toughness.
  • FREVATM SES60 composited by non-halogen flame retardant polymer, which can resist >1000 °C blaze flame for more than 60 minutes with a thickness of 0.6mm. According to our test, after 1 hour burning, FREVATM SES60 can still maintain its structural strength without break.
  • FREVATM SES60 is halogen-free, formaldehyde-free and toluene-free. When it is burned, most of the emission is water vapor with very low smoke.
  • FREVATM SES60 is a good replacement of fireproof fabric for passive fire protection systems, such as fire/smoke curtains, fire shutters.

Information provided by USI Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 600 microns23.6 milTotal
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 0.785 MPa114 psi
Elongation at Break 30 %30 %
 
Descriptive Properties
Basis Weight960 g/m2
Length100m
 50m
Width1200mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PUSIC042 / 285410

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.