MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Parker Chomerics Tecknit NC-Consil® 770 Nickel Coated Graphite Filled Silicone Elastomer
Categories: Polymer; Thermoset; Silicone

Material Notes: Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil is designed to provide reliable cost effective shielding for a wide range of EMI applications ideal for the commercial market.

Typical Applications: NC-Consil should be used where there is a need for high broadband shielding combined with excellent environmental sealing properties.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.74 - 2.26 g/cc1.74 - 2.26 g/ccASTM D792
Deformation 10 %10 %5 pli
 20 %20 %10 pli
 30 %30 %25 pli
 50 %50 %85 pli
 60 %60 %155 pli
 65 %65 %205 pli
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 60 - 8060 - 80ASTM D2240
Tensile Strength >= 1.03 MPa>= 150 psiASTM D412
Elongation at Break >= 100 %>= 100 %ASTM D412
Tear Strength 8.77 kN/m50.0 pliASTM D624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 0.10 ohm-cm<= 0.10 ohm-cm
Shielding Effectiveness  85 dB
@Frequency 1e+10 Hz
85 dB
@Frequency 1e+10 Hz
Plane Wave
 100 dB
@Frequency 100000 Hz
100 dB
@Frequency 100000 Hz
H-Field
 100 dB
@Frequency 1e+7 Hz
100 dB
@Frequency 1e+7 Hz
E-Field
 100 dB
@Frequency 1e+9 Hz
100 dB
@Frequency 1e+9 Hz
Plane Wave
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 160 °C320 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Descriptive Properties
BinderSilicone
ColorDark Gray
FillerNickel Coated Graphite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics Tecknit Consil®-E 811 Extruded Silver-Filled Silicone Elastomer
Parker Chomerics Tecknit Consil®-A 895 Silver-Aluminum Filled Silicone Elastomer
Parker Chomerics Tecknit Consil®-C 871 Silver-Copper Filled Silicone Elastomer
Parker Chomerics Tecknit Consil®-E 815 Extruded Silver-Filled Silicone Elastomer
Parker Chomerics Tecknit NC-Consil® FR751 Nickel Coated Graphite Filled Silicone Elastomer

PCHOME388 / 131098

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.