MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LATI Lapex A G/20 PES, 20% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyethersulfone (PES); Polyethersulfone (PES), 20%Glass Fiber Filled

Material Notes: Polyether Sulfone (PES) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stability.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.49 g/cc
Linear Mold Shrinkage, Flow 0.0035 - 0.0050 cm/cm
Linear Mold Shrinkage, Transverse 0.0075 - 0.0090 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPa
@Temperature 150 °C
 90.0 MPa
@Temperature 120 °C
 100 MPa
@Temperature 90.0 °C
 110 MPa
@Temperature 60.0 °C
 115 MPa
@Temperature 23.0 °C
Elongation at Break 2.5 %
@Temperature 23.0 °C
 2.6 %
@Temperature 60.0 °C
 2.7 %
@Temperature 90.0 °C
 2.8 %
@Temperature 120 °C
 3.0 %
@Temperature 150 °C
Elongation at Yield 2.5 %
@Temperature 150 °C
Tensile Modulus 5900 MPa
@Temperature 150 °C
 6150 MPa
@Temperature 120 °C
 6300 MPa
@Temperature 90.0 °C
 6500 MPa
@Temperature 60.0 °C
 6700 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched 35.0 kJ/m²
Charpy Impact, Notched 4.00 kJ/m²
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °C
Deflection Temperature at 0.46 MPa (66 psi) 220 °C
Deflection Temperature at 1.8 MPa (264 psi) 215 °C
Vicat Softening Point 220 °C
@Load 5.00 kg
Flammability, UL94 V-0
@Thickness 3.00 mm
 V-0
@Thickness 1.50 mm
Oxygen Index 39 %
 
Processing PropertiesOriginal ValueComments
Melt Temperature 350 - 370 °C
Mold Temperature 140 - 165 °C
Drying Temperature 150 - 180 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultrason® E 2010 G4 20% Glass Filled PES
Gharda Chemicals GAFONE™ 3420GF PES, Glass Fiber-Reinforced
RTP Company RTP 1403 Polyethersulfone (PES), Glass Fiber
Techmer ES HiFill® PES GF20 20% Glass Filled
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled

PLATH9614 / 177310

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.