MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

CIPLAS PRF3500J Polypropylene Homopolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Product Description: PRF3500J is a high melt random copolymer with fast cycle time and easy mold release. It is designed for injection molding including thin wall applications. Its clarity makes it an excellent choice for "see-through" housewares and rigid packaging product dimensional stability.

Applications:

  • Thin-wall Food Container
  • Stationary
  • CD/DVD cases

Information provided by CIPLAS by ITOCHU

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 35 g/10 min
@Temperature 230 °C
35 g/10 min
@Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 100100ASTM D785
Tensile Strength, Yield 29.6 MPa4300 psi50mm/min; ASTM D638
Elongation at Yield 13 %13 %50mm/min; ASTM D638
1% Secant Modulus 1070 MPa155000 psiFlexural, 1.3mm/min; ASTM D790
Izod Impact, Notched 0.481 J/cm0.900 ft-lb/inASTM D256
 
Optical PropertiesMetricEnglishComments
Haze 15 %15 %Plaque; FTTC 5606

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCIPLA042 / 284020

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.