MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Avient Versalloy™ HC 9220-90 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Versalloy™ HC 9220-90 is a TPV alloy targeted for extrusion and injection molding healthcare applications such as medical tubing, disposable medical items and soft-touch overmolding for surgical grips. Product exhibits exceptional flow properties and surface aesthetics. * Excellent Extrudability * Good Flow for Injection Molding * Exceptional Colorability * Overmold Adhesion to Polypropylene * Superior Surface Aesthetics

Versalloy™ HC 9220-90 can be recycled as a filler or impact modifier for polyolefins, or can be recycled by grinding and reintroduction to the molding process. Similar to PP or PE recycling process, if separated appropriately, it can be recycled many times. Municipality waste stream recycle code is 7 which is designated for Other. Please contact GLS Thermoplastic Elastomers for a copy of our Recyclability Compliance letter.

Color concentrates with polypropylene (PP) carrier are most suitable for coloring Versalloy™ HC 9220-90. Improved color dispersion can be achieved by using higher melt flow concentrates (with a melt flow from 25 - 40 g/10 min). Typical loadings for color concentrates are 1% to 5% by weight. Concentrates based on PVC should not be used. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). Regrind levels up to 20% can be used with Versalloy™ HC 9220-90 with minimal property loss, provided that the regrind is free of contamination. To minimize losses during molding, the melt temperature should remain as low as possible. The final determination of regrind effectiveness should be determined by the customer. Versalloy™ HC 9220-90 has good melt stability. Empty the barrel for idle periods of fifteen (15) minutes or longer. Injection Speed: 1 to 5 in/sec 1st Stage - Boost Pressure: 300 to 700 psi 2nd Stage - Hold Pressure: 30% of Boost Hold Time (Thick Part): 4 to 10 sec Hold Time (Thin Part): 1 to 3 sec

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.933 g/cc0.933 g/ccASTM D792
Viscosity 28600 cP
@Shear Rate 11200 1/s,
Temperature 200 °C
28600 cP
@Shear Rate 11200 1/s,
Temperature 392 °F
ASTM D3835
Linear Mold Shrinkage, Flow 0.021 cm/cm0.021 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.019 cm/cm0.019 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 909010 sec; ASTM D2240
Tensile Strength at Break  13.0 MPa
@Temperature 21.0 °C
1890 psi
@Temperature 69.8 °F
Die C Flow 2 hr; ASTM D412
 13.9 MPa
@Temperature 23.0 °C
2020 psi
@Temperature 73.4 °F
Die C Across Flow 2 hr; ASTM D412
Tensile Stress at Strain  7.10 MPa
@Strain 100 %,
Temperature 21.0 °C
1030 psi
@Strain 100 %,
Temperature 69.8 °F
Across Flow 2 hr; ASTM D412
 8.16 MPa
@Strain 300 %,
Temperature 23.0 °C
1180 psi
@Strain 300 %,
Temperature 73.4 °F
Die C Across Flow 2 hr; ASTM D412
 9.16 MPa
@Strain 100 %,
Temperature 21.0 °C
1330 psi
@Strain 100 %,
Temperature 69.8 °F
Die C Flow 2 hr; ASTM D412
 10.5 MPa
@Strain 300 %,
Temperature 21.0 °C
1520 psi
@Strain 300 %,
Temperature 69.8 °F
Die C Flow 2 hr; ASTM D412
Elongation at Break  540 %
@Temperature 21.0 °C
540 %
@Temperature 69.8 °F
Die C Flow 2 hr; ASTM D412
 700 %
@Temperature 23.0 °C
700 %
@Temperature 73.4 °F
Die C Across Flow 2 hr; ASTM D412
Tear Strength 67.4 kN/m385 pliAcross Flow; ASTM D624
 72.4 kN/m413 pliFlow; ASTM D624
Compression Set  25 %
@Temperature 23.0 °C,
Time 79200 sec
25 %
@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
 25 %
@Temperature 23.0 °C,
Time 605000 sec
25 %
@Temperature 73.4 °F,
Time 168 hour
ASTM D395B
 41 %
@Temperature 70.0 °C,
Time 79200 sec
41 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395B
 55 %
@Temperature 100 °C,
Time 79200 sec
55 %
@Temperature 212 °F,
Time 22.0 hour
ASTM D395B
 59 %
@Temperature 70.0 °C,
Time 605000 sec
59 %
@Temperature 158 °F,
Time 168 hour
ASTM D395B
 69 %
@Temperature 100 °C,
Time 605000 sec
69 %
@Temperature 212 °F,
Time 168 hour
ASTM D395B
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 177 - 193 °C351 - 379 °F
Middle Barrel Temperature 182 - 218 °C360 - 424 °F
Front Barrel Temperature 193 - 218 °C379 - 424 °F
Nozzle Temperature 193 - 224 °C379 - 435 °F
Zone 1 166 - 182 °C331 - 360 °F
Zone 2 177 - 204 °C351 - 399 °F
Zone 3 182 - 216 °C360 - 421 °F
Die Temperature 182 - 210 °C360 - 410 °F
Mold Temperature 15.6 - 26.7 °C60.1 - 80.1 °F
Drying Temperature 80.0 °C176 °F
 80.0 °C176 °F
Dry Time 3.00 hour3.00 hour
 3.00 hour3.00 hour
Back Pressure 0.000 - 0.689 MPa0.000 - 99.9 psi
Screw Speed 50 - 100 rpm50 - 100 rpm
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes
 
Descriptive Properties
Agency RatingsISO 10993 Part 4
 ISO 10993 Part 5
AppearanceNatural Color
FeaturesGood Colorability
 Good Processability
 Good Surface Finish
 Non-Phthalate Plasticizer
 Recyclable Material
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodExtrusion
 Injection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
Suggested Max Regrind20%
UsesFlexible Grips
 Medical/Healthcare Applications
 Overmolding
 Soft Touch Applications
 Tubing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber
Avient Versalloy™ HC 9220-70 Thermoplastic Elastomer (TPE)
Advanced Elastomer Systems Santoprene® 281-64 Thermoplastic Rubber
Advanced Elastomer Systems Santoprene® 283-40 Thermoplastic Rubber
Avient Dynaflex™ G2706-1000-00 Thermoplastic Elastomer (TPE)

PH0POL1349 / 145918

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.