MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Dow Sylgard® 3-6605 Thermally Conductive Silicone Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: Former Dow Corning product.

Information provided by Dow Corning

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.14 g/cc
Viscosity 47000 cPdynamic
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 78
Tensile Strength, Ultimate 850 psi
Elongation at Break 90 %
Shear Strength 350 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cm
Dielectric Constant 4.5
@Frequency 100000 Hz
 4.51
@Frequency 100 Hz
Dielectric Strength 455 V/mil
Dissipation Factor <= 0.0010
@Frequency 100000 Hz
 0.0058
@Frequency 100 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 225 µm/m-°C
Thermal Conductivity 0.850 W/m-K
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -45.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 15.0 min
@Temperature 150 °C
heat cure
 45.0 min
@Temperature 125 °C
heat cure
 90.0 min
@Temperature 100 °C
heat cure
Shelf Life 12.0 Month
 
Descriptive Properties
Colorgrey
Flowableyes
Hydrophobicyes
Mix Ratio (X:1)100Base to Catalyst
Self Levelingyes
Water Resistantyes
Working Time (min)>1440

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shin-Etsu Silicones X-65-130U Electrically Conductive Silicone Elastomer
Wacker Elastosil® LR 3141/50 A/B Liquid Silicone Rubber
Celanese Nilit FRIANYL B63 AL40 Nylon 6.6 for injection molding, 40% aluminum filled
Abatron L060421-1 Heat-Resistant Non-Flammable Silicone Rubber
Momentive Performance Materials XE20-A7016U Heat Cured Rubber - Thermal Conductive

PDOWCO580 / 106281

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.