MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

American Red Western Cedar (Giant Arborvitae) Wood
Categories: Wood and Natural Products; Wood; Softwood

Material Notes: An acidic timber which may corrode metals under damp conditions and cause iron staining. Conifer
Usual surface texture: Coarse
Dimensional changes when dried lumber is subjected to variations in humidity during service: Small
Resistance to fungal decay (Heartwood in ground contact): Durable (15 to 25 years)
Resistance to penetration by preservatives: Resistant
Common Applications: Shingles, exterior cladding, greenhouses, beehives

Property values marked by an asterisk (*) have been taken from an unusually old reference source.

Key Words: Thuja plicata; Lumber, Timber
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.310 g/cc0.0112 lb/in³Oven Dry Weight/Unseasoned Volume
 0.330 g/cc0.0119 lb/in³Air Dry (12-15% Moisture Content)
 0.433 g/cc0.0156 lb/in³Unseasoned*
Moisture Absorption at Equilibrium 1.5 - 8.0 %1.5 - 8.0 %Between 40% RH and 90% RH
Cell Length 7.00 mm0.276 inMature Wood
 
Mechanical PropertiesMetricEnglishComments
Hardness, Wood Indentation 1200 N270 lb (f)Side. Force required to imbed a 0.444 inch steel ball to one-half its diameter
 1600 N360 lb (f)Side
 1900 N427 lb (f)End. Force required to imbed a 0.444 inch steel ball to one-half its diameter
Tensile Strength, Ultimate 1.50 MPa218 psiPerpendicular to Grain
Modulus of Rupture 0.0359 GPa5.20 ksiStatic Bending*
 0.0530 GPa7.69 ksiStatic Bending
Flexural Yield Strength 22.8 MPa3300 psiFiber Stress at Elastic Limit; Static Bending*
Flexural Modulus 6.55 GPa950 ksiStatic Bending*
 7.73 GPa1120 ksiStatic Bending
Compressive Strength 2.14 MPa310 psiPerpendicular to Grain*
 4.20 MPa609 psiPerpendicular to Grain
 17.2 MPa2500 psiParallel to Grain*
 19.6 MPa2840 psiMax Crushing Strength Parallel to Grain*
 43.0 MPa6240 psiParallel to Grain
Poissons Ratio 0.2960.296µLT, 12% Moisture Content
 0.3780.378µLR, 12% Moisture Content
 0.4030.403µTR, 12% Moisture Content
 0.4840.484µRT, 12% Moisture Content
Machinability 100 %100 %Good Relative to Other Wood
Shear Strength 4.96 MPa720 psiParallel to Grain*
 5.90 MPa856 psiOrientation Unknown
Impact 2.42.4in-lb/in³; Work to Elastic Limit; Unseasoned Sample; Impact Bending*
 71007100psi; Fiber Stress at Elastic Limit; Unseasoned Sample; Impact Bending*
Work to Elastic Limit 0.00441 J/cm³0.640 in-lb/in³Static Bending*
Work to Maximum Load 0.0345 J/cm³5.00 in-lb/in³Static Bending*
Toughness 10.2 J7.52 ft-lbRadial
 14.7 J10.8 ft-lbTangential
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.0821 W/m-K0.570 BTU-in/hr-ft²-°FOven Dry
 0.0980 W/m-K0.680 BTU-in/hr-ft²-°F12% Moisture Content
Shrinkage 2.4 %2.4 %Radial; Green to Zero Moisture
 2.4 %2.4 %Tangential; Unseasoned to Oven Dry*
 4.4 %4.4 %Tangential; Green to Zero Moisture
 6.8 %6.8 %Volumetric; Green to Zero Moisture
 7.6 %7.6 %Radial; Unseasoned to Oven Dry*
 23 %23 %Volumetric; Unseasoned to Oven Dry*
 
Descriptive Properties
ColorReddish brownUsual for heartwood

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
American Red Spruce Wood
Red Pine Wood
American Northern White Cedar (Eastern Arborvitae) Wood
American Sitka Spruce Wood
American Balsam Fir Wood

PTSA550 / 71262

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.