A hybrid moldable resin material PIOCLEAN, consisting of polystyrene and polyolefin, achieves performance exceeding that of the individual components by effectively combining materials with drastically different characteristics. Major use of Molded articles: General molded articles Information provided by Sekisui Plastic Co. Ltd. |