MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

MRC Polymers NAXELL™ PC110MH-202 Medium/High MFR Polycarbonate  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Mechanical properties measured on 1/8 in. (3.2 mm) samples.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption 0.15 %0.15 %24 hr.; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 17 g/10 min
@Load 1.20 kg,
Temperature 300 °C
17 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 62.0 MPa8990 psiASTM D638
Elongation at Break 70 %70 %ASTM D638
Flexural Strength 96.0 MPa13900 psiASTM D790
Flexural Modulus 2.343 GPa339.8 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
CTE, linear 67.5 µm/m-°C
@Temperature -40.0 - 35.0 °C
37.5 µin/in-°F
@Temperature -40.0 - 95.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 135 °C275 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C264 °FUnannealed; ASTM D648
Flammability, UL94  HB
@Thickness 1.47 mm
HB
@Thickness 0.0579 in
MRC Rating
 V-2
@Thickness 3.20 mm
V-2
@Thickness 0.126 in
MRC Rating
 
Processing PropertiesMetricEnglishComments
Processing Temperature 275 - 291 °C527 - 556 °F
Rear Barrel Temperature 255 - 271 °C491 - 520 °F
Middle Barrel Temperature 265 - 280 °C509 - 536 °F
Front Barrel Temperature 275 - 291 °C527 - 556 °F
Nozzle Temperature 275 - 291 °C527 - 556 °F
Mold Temperature 49.0 - 93.0 °C120 - 199 °F
Drying Temperature 116 °C241 °F
Dry Time 3 - 4 hour3 - 4 hour
Moisture Content <= 0.020 %<= 0.020 %
Dew Point <= -17.8 °C<= 0.000 °F
Drying Air Flow Rate 22.7 - 28.3 l/min0.800 - 1.00 ft³/min (CFM)per lb/hour or resin processes
Injection Pressure 68.9 - 138 MPa10000 - 20000 psi
Back Pressure 0.345 - 1.21 MPa50.0 - 175 psi
Cushion 0.635 cm0.250 in
Screw Speed 50 - 75 rpm50 - 75 rpm
 
Descriptive Properties
Fill RateModerate
Hold40 - 60% of injection pressure
Packing50 - 75% of injection pressure

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMRC962 / 21019

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.