MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil Bicor® 120 CSR-2 OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: Bicor CSR-2 is a one-side treated OPP film designed for cold seal release, either unsupported or as the outer web of a lamination.

Availability: Latin America, North America and South America

Key Features:

  • Excellent cold seal adhesion and ink adhesion on the treated surface
  • Non-migratory slip system for consistent COF
  • Excellent release from cold seal adhesives
Applications:
  • Bakery
  • Biscuits/Cookie/Crackers
  • Confectionery, Chocolate
  • Dairy Products
  • Fresh Produce
Uses:
  • HFFS Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive, Outer Web Adhesive Lamination, Outer Web Extrusion Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission 4.30 g/m²/day
@Temperature 38.0 °C
90% RH; ExxonMobil Method
Thickness 1.20 milNominal; ExxonMobil Method
Coating Weight 17.1 lb/reamExxonMobil Method
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction 0.20slip modified; ExxonMobil Method
Film Tensile Strength at Break, MD 18000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 35000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Shrinkage, MD 4.0 %
@Temperature 135 °C
ExxonMobil Method
Shrinkage, TD 4.0 %
@Temperature 135 °C
ExxonMobil Method
 
Optical PropertiesOriginal ValueComments
Haze 2.0 %ExxonMobil Method
Gloss 88 %45°, Untreated Surface; ExxonMobil Method
 
Descriptive Properties
Wetting Tension0.83 receding COS thetaTreated Surface
Yield25200 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEXB424 / 37729

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.