MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Manufacturing Insight EFR-3 Enhanced Fire Retardant Additive  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: EFR-3 is ideal for incorporation into unreinforced thermoset resin systems, including coatings and foams, potting compounds as well as electronic laminates and other similar applications. EFR-3 has been proven especially successful in phenolic matrices, but also functions well in epoxy and urethane resin systems.

When blended into a resin system, EFR-3 will react to heat and/or flame by foaming and forming a thick, high yield char barrier. The char barrier will extinguish fire and prevent further flame spread. Additionally, the char foam insulates and protects the polymer substrate from heat and fire damage.

EFR-3 is halogen-free, contains no metals, PBDEs, PBBs or other brominated compounds and does not evolve the highly toxic and corrosive gasses associated with many other fire retardant compounds. EFR-3 is a RoHS/WEEE compliant material. EFR-3 functions at loading levels in the range of 10%-20% by weight. Flame spread and smoke developed values (ASTM E-84) are typically 10/10 and under and are in compliance with UL 94V0, MSC.41 (64) and FAR 25.853.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solubility in Water <= 1.0 %<= 1.0 %At 170°F
Particle Mesh Size 325 Mesh325 Mesh100% through
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0
 
Descriptive Properties
AppearanceVery fine free flowing white powder
Char Activation Temp300°C
Char Forming Efficiency99% Minimum
Purity98% Minimum

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMFGINS3 / 52931

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.