MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Avient Nymax™ 604 Black Nylon 6  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes: This product is a fully compounded, industrial grade nylon 6. It has been developed for applications where low cost is the primary driver. Ease of processing and consistent physical properties are some of the benefits of this grade.

Property data measured on molded test bars: Dry as Molded

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
Water Absorption 1.5 %
@Time 86400 sec
1.5 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0080 - 0.011 cm/cm0.0080 - 0.011 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 74.1 MPa10700 psiType I; ASTM D638
Elongation at Yield 25 %25 %Type I, 5.1 mm/min; ASTM D638
Flexural Yield Strength 110 MPa16000 psiASTM D790
Flexural Modulus 2.76 GPa400 ksiASTM D790
Izod Impact, Notched 0.534 J/cm
@Thickness 1.57 mm,
Temperature -40.0 °C
1.00 ft-lb/in
@Thickness 0.0618 in,
Temperature -40.0 °F
Across Flow, Compression Molded; ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Melting Point 216 °C421 °FASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 57.2 °C
@Thickness 1.57 mm
135 °F
@Thickness 0.0618 in
Annealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 282 °C540 °F
Mold Temperature 65.6 - 93.3 °C150 - 200 °F
Drying Temperature 71.1 - 82.2 °C160 - 180 °F
 
Descriptive Properties
FormsPellets
Generic NamePolyamide 6 (Nylon 6)
Regional AvailabilityNorth America
 South America
UsesIndustrial Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PH1PN9288 / 103124

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.