Hostacom HKG743T BLK 40% glass/mineral-reinforced polypropylene homopolymer has exceptional stiffness and good dimensional stability. It is typically used as a potential replacement for more costly engineering thermoplastics. Typical applications include automotive under hood components, instrument panel substrates, and electronic housings. Applications: Interior Automotive ApplicationsInformation provided by LyondellBasell. |