MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® 5714 Ether Based Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: Low Temperature Flexibility, Excellent Abrasion, Fungal, and Chemical Resistance, and Hydrolytic Stability. Adhesives can be applied from solution or extruded as a melt coating. The resin is lightly dusted with calcium stearate and contains UV stabilizer.

Uses: Various adhesive and fabric coating, magnetic media binder and cast films for lamination

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Noveon, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Viscosity 72000 cP
@Temperature 204 °C
ASTM D-1084-88
Brookfield Viscosity 900 cPRVT Spindle #2, 20 RPM, 23°C, 15% T.S. in THF
 3700 cPRVT Spindle #2, 20 RPM, 23°C, 15% T.S. in Cyclohexanone
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 80ASTM D2240
Tensile Strength 31.0 MPaASTM D412/D638
Elongation at Break 530 %ASTM D412/D638
100% Modulus 0.00480 GPa
@Strain 100 %
ASTM D412/D638
300% Modulus 0.00900 GPa
@Strain 300 %
ASTM D412/D638
Peel Strength 0.500 kN/mASTM D-1876-72
 1.50 kN/mASTM D-1876-72
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 160 °FASTM D1525
Glass Transition Temp, Tg -38.0 °CDSC
Ring & Ball Softening Point 174 °CASTM E-28-92
 
Descriptive Properties
Gradient Bar Tack Temperature127°C
Open Time<5 secASTM D-4497-94

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 5715 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 5708 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane
Lubrizol ESTANE® 5703 Ester Based Thermoplastic Polyurethane

PNOVEON015 / 55280

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.