MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Borealis Borstar® LE6027 LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Borstar® LE6027 is a black linear low density polyethylene compound, which is produced with the Borealis proprietary Borstar bimodal process technology. It is characterized by excellent stress crack resistance and mechanical properties and low temperature performance in combination with good extrudability and flexibility. Borstar® LE6027 contains 2,5 % well dispersed furnace black in order to ensure excellent weathering resistance

Applications: Jackets for energy and communication cables

Typical characteristics:

  • Excellent environmental stress-cracking resistance (ESCR)
  • Low shrinkage
  • Excellent mechanical properties
  • Very good UV resistance
  • Good flexibility
  • Good petroleum-jelly resistance
  • Low water permeability
Specifications: Borstar® LE6027 is expected to meet the applicable requirements included in the below mentioned standards provided it is processed using sound material handling and processing practices as well as appropriate testing procedures. EN 50290-2-24 HD 620 S2 DMP 9, 10, 12, 14, 15, 17; HD 603 S1 DMP 5, 7, 8. Cables manufactured with Borstar® LE6027 using sound extrusion practice normally comply with the following cable product standards: IEC 60708; IEC 60502, Part 2, Type ST3, ST7; IEC 60840, Type ST3, ST7; HD 632 S2, ST3, ST7; EN 187105

Information provided by Borealis AG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.921 g/ccBase resin; ISO 1183-1
 0.933 g/ccISO 1183-1
ESCR 10% Igepal® >= 2500 hour
@Temperature 50.0 °C
IEC 60811-406
Melt Flow 0.900 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133-1
Storage Temperature 10.0 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 52.0
@Time 1.00 sec
ISO 868
Tensile Strength 25.0 MPa25 mm/min; ISO 527-2
Elongation at Break <= 750 %25 mm/min; ISO 527-2
Flexural Modulus 370 MPaISO 178
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 10.0 ohm-cmIEC 60093
Dielectric Strength >= 20.0 kV/mmIEC 60243
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBORE9677 / 323034

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.