MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

UBE 1015GX78V Polyamide 6, Glass Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Heat Stabilized

Material Notes: Characteristic: Injection, reinforced with glass fiber 33%, heat and UV stabilized, black color.

Information provided by UBE Industries, LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³ISO 1183-3
Moisture Absorption 1.80 %1.80 %50% RH; UBE method
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 3.00 mm
0.0020 in/in
@Thickness 0.118 in
30x100x3t; UBE method
Linear Mold Shrinkage, Transverse 0.0070 cm/cm
@Thickness 3.00 mm
0.0070 in/in
@Thickness 0.118 in
30x100x3t; UBE method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 185 MPa26800 psiISO 527-1,2
Elongation at Break 2.5 %2.5 %ISO 527-1,2
Tensile Modulus 10.5 GPa1520 ksiISO 527-1,2
Flexural Strength 270 MPa39200 psiISO 178
Flexural Modulus 9.80 GPa1420 ksiISO 178
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²ISO 179-1/1eA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 400 - 600 V400 - 600 VUL746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear 2.50 µm/m-°C1.39 µin/in-°FISO 11359-2
Melting Point 215 - 225 °C419 - 437 °FISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75-1,2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75-1,2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PUBD9822 / 287285

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.