MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Tritan™ Renew LX151HF-30 Copolyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Tritan™ Renew LX151HF-30 is a high flow grade of an amorphous copolyester with excellent appearance and clarity. Tritan Renew LX151HF-30 has viscosity reductions of 40-50% relative to standard grades of Eastman Tritan. Tritan Renew LX151HF-30 contains a mold release derived from vegetable based sources. Its most outstanding features are excellent toughness, hydrolytic stability, and heat and chemical resistance. Tritan Renew LX151HF-30 was developed for the cosmetic, fragrance, and personal care markets. Tritan Renew LX151HF-30can easily be converted into articles for application in consumer and personal care markets by injection molding, extrusion blow molding, and injection blow molding. Eastman Renew polymers have been certified by International Sustainability & Carbon Certification (ISCC), a global, independent agency for tracking sustainable content in a variety of industries. Renew polymers are produced with ISCC certified circular content by mass balance allocation.

Applications

  • Bottles-fragrance pkg
  • Closures-fragrance pkg
  • Color cosmetics packaging
  • Fragrance packaging
  • Personal care & cosmetics packaging
  • Personal care bottles
  • Personal care packaging
  • Skin care packaging
Key Attributes
  • Ease of processing
  • Excellent clarity
  • Fast drying times
  • Good chemical resistance
  • Good heat resistance
  • Improved flowability
  • Outstanding impact resistance
  • Quick cycle times

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccASTM D792
Linear Mold Shrinkage 0.00500 - 0.00700 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 111ASTM D785
Tensile Strength at Break 52.0 MPaASTM D638
Tensile Strength, Yield 43.0 MPaASTM D638
Elongation at Break 210 %ASTM D638
Elongation at Yield 7.00 %ASTM D638
Tensile Modulus 1575 MPaASTM D638
Flexural Yield Strength 64.0 MPaASTM D790
Flexural Modulus 1575 MPaASTM D790
Izod Impact, Notched 110 J/m
@Temperature -40.0 °C
ASTM D256
 860 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched NB
@Temperature 23.0 °C
ASTM D4812
 NB
@Temperature -40.0 °C
ASTM D4812
Puncture Energy 53.0 J
@Temperature 23.0 °C
@ Max. Load; ASTM D3763
 57.0 J
@Temperature -40.0 °C
@ Max. Load; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze <= 1.00 %ASTM D1003
Transmission, Visible 91.0 %Total; ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 - 282 °C
Mold Temperature 38.0 - 66.0 °C
Drying Temperature 88.0 °C
Dry Time 4.00 - 6.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4214 / 323837

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.