MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Evonik VESTAKEEP® 50001XT BK PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Unreinforced

Material Notes: VESTAKEEP® 50001XT BK is a high viscosity, unreinforced, unlubricated polyether ether ketone for injection molding and extrusion and can be cross-linked after processing by heat treatment. The semi-crystalline polymer features superior property retention at elevated temperatures combined with the chemical resistance of standard PEEK. Parts made from VESTAKEEP® 50001XT BK feature a very high resistance to creep. VESTAKEEP® 50001XT BK can be processed by common machines for PEEK processing. VESTAKEEP® 50001XT BK is supplied as granules in 25 kg boxes with moisture-proof polyethylene liners. As VESTAKEEP® 50001XT BK is a reactive system the manufacturer recommends low melt temperatures and short cycle times. Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C. Preliminary data sheet.
Dry properties listed below
Industrial Sector: Energy, Oil and Gas
Processing: Injection molding
Delivery form: Pellets, Granules
Resistance to: Heat (thermal stability), Fire / burn
Special Characteristics: Semi-crystalline, Crosslinkable, High viscosity
Features: Creep resistance, Low coefficient of friction
Color: Black

Information provided by Evonik.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³ISO 1183
Melt Flow 7.40 g/10 min
@Load 5.00 kg,
Temperature 380 °C
7.40 g/10 min
@Load 11.0 lb,
Temperature 716 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 90.0
@Time 1.00 sec
90.0
@Time 0.000278 hour
annealed; ASTM D2240
Coefficient of Friction 0.2700.270ISO 7148-2
K (wear) Factor 2.00 x 10-8 mm³/N-M
@Pressure 4.00 MPa
0.993 x 10-10 in³-min/ft-lb-hr
@Pressure 580 psi
parallel, Test speed: 0.5 m/s; ISO 7148-2
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 °C352 °FASTM D3418
Glass Transition Temp, Tg 178 °C352 °FISO 11357-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 357 °C675 °FInjection Molding; ISO 294
Mold Temperature >= 218 °C>= 424 °FInjection Molding; ISO 294
Injection Velocity 200 mm/sec7.87 in/secInjection Molding; ISO 294
Moisture Content 0.0400 %0.0400 %ISO 15512
 
Descriptive Properties
Colorblack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEVONIK7840 / 324972

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.