MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Parker Chomerics CHO-JAC CJ-022 Flat Cable EMI Shield
Categories: Other Engineering Material

Material Notes: Flat Cable EMI Shield. Cho-Jack® shielding is a high quality flat cable jacket designed to attenuate RF signals and bring digital electronic devices into compliance with FCC and TEMPEST radiated emissions limits as well as EU and MIL-STD radiated emissions and susceptibility limits.

Information provided by Chomerics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 25.4 microns1.00 milPolyester Film
 35.6 microns1.40 milCopper Foil
 88.9 microns3.50 milTotal; ASTM D1000
 
Mechanical PropertiesMetricEnglishComments
Tear Strength, Total 11.12 N2.500 lb (f)
 
Electrical PropertiesMetricEnglishComments
Shielding Effectiveness  -100 dB
@Frequency 600 Hz
-100 dB
@Frequency 600 Hz
 -10.0 dB
@Frequency 140 Hz
-10.0 dB
@Frequency 140 Hz
 -7.00 dB
@Frequency 230 Hz
-7.00 dB
@Frequency 230 Hz
 -5.00 dB
@Frequency 200 Hz
-5.00 dB
@Frequency 200 Hz
 5.0 dB
@Frequency 400 Hz
5.0 dB
@Frequency 400 Hz
 5.0 dB
@Frequency 100 Hz
5.0 dB
@Frequency 100 Hz
 12 dB
@Frequency 900 Hz
12 dB
@Frequency 900 Hz
 25 dB
@Frequency 40.0 Hz
25 dB
@Frequency 40.0 Hz
 50 dB
@Frequency 1e+9 Hz
50 dB
@Frequency 1e+9 Hz
With 360° ground termination
 55 dB
@Frequency 4.00e+8 Hz
55 dB
@Frequency 4.00e+8 Hz
With 360° ground termination
 73 dB
@Frequency 1e+8 Hz
73 dB
@Frequency 1e+8 Hz
With 360° ground termination
 75 dB
@Frequency 4.00e+7 Hz
75 dB
@Frequency 4.00e+7 Hz
With 360° ground termination
Dielectric Strength 177 kV/mm4500 kV/inWith 360° ground termination
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 105 °C221 °F
Flammability, UL94 V-0V-0
 
Descriptive Properties
Adhesion of Foil to Insulator4 lbs/in
Adhesion of Sealing adhesive2.5 lbs/in
FlexibilityPassIPC-TM-650 Method 2.4.5
GradeCommercial

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics V-THERM™ Thermally Conductive Elastomer
Parker Chomerics SOFT-SHIELD® 5500 EMI Shielding and Grounding Gasket
Parker Chomerics CHO-MUTE 9020 RF Absorber
Parker Chomerics CHO-FORM 5537 EMI Shielding Material
Parker Chomerics CHO-BOND® 586 Conductive Epoxy

PCHOME092 / 28314

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.