MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Rogers Arlon DiClad 880 PTFE/Woven Fiberglass Laminate
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes:
  • Extremely Low Loss Tangent
  • Excellent Dimensional Stability
  • Product Performance Uniformity

Benefits:

  • Electrical Properties are highly uniform across frequency
  • Consistent Mechanical Performance
  • Excellent Chemical Resistance

Typical Applications:

  • Military Radar Feed Networks
  • Commercial Phased Array Networks
  • Low Loss Base Station Antennas
  • Missile Guidance Systems
  • Digital Radio Antennas
  • Filters, Couplers, LNAs

Information provided by Arlon Materials for Electronics (MED); now a part of Rogers Corporation.

Vendors: Arlon Materials for Electronics (MED) is a major manufacturer of specialty high performance laminate and prepreg materials for use in a wide variety of printed circuit board (PCB) applications and in several distinctive markets.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.23 g/ccASTM D792 Method A
Water Absorption 0.020 %IPC TM-650 2.6.2.2
Outgassing - Total Mass Loss 0.010 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
Water Vapor Recovered; NASA SP-R-0022A
 0.010 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
NASA SP-R-0022A
Collected Volatile Condensable Material 0.010 %
@Pressure <=1.33e-10 MPa,
Temperature 125 °C
NASA SP-R-0022A
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 7500 psiCross; ASTM D882
 8100 psiMachine; ASTM D882
Modulus of Elasticity 202 ksiCross; ASTM D638
 267 ksiMachine; ASTM D638
Flexural Modulus >= 357 ksiASTM D790
Compressive Modulus 237 ksiASTM D695
Peel Strength 14.0 pliAfter Thermal Stress; IPC TM-650 2.4.8
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.40e+15 ohm-cmC96/35/90; IPC TM-650 2.5.17.1
Surface Resistance 2.90e+12 ohmC96/35/90; IPC TM-650 2.5.17.1
Dielectric Constant 2.17 - 2.2
@Frequency 1e+6 Hz
C23/50; IPC TM-650 2.5.5.3
 2.17 - 2.2
@Frequency 1e+10 Hz
C23/50; IPC TM-650 2.5.5.5
Dielectric Breakdown >= 45000 VD48/50; ASTM D149
Dissipation Factor 0.00080
@Frequency 1e+6 Hz
C23/50; IPC TM-650 2.5.5.3
 0.00090
@Frequency 1e+10 Hz
C23/50; IPC TM-650 2.5.5.5
Arc Resistance >= 180 secD48/50; ASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear 25.0 µm/m-°C
@Temperature 0.000 - 100 °C
x direction; IPC TM-650 2.4.24
 34.0 µm/m-°C
@Temperature 0.000 - 100 °C
y direction; IPC TM-650 2.4.24
CTE, linear, Transverse to Flow 252 µm/m-°C
@Temperature 0.000 - 100 °C
z direction; IPC TM-650 2.4.24
Thermal Conductivity 0.261 W/m-K
@Temperature 100 °C
ASTM E1225
Flammability, UL94 V-0Vertical Burn
 
Descriptive Properties
Temperature Coefficient of Dielectric (ppm/°C)-160IPC TM-650 2.5.5.5 (-10 - 140°C)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Arlon DiClad 522/527 PTFE/Woven Fiberglass Laminates
Rogers Arlon DiClad 870 PTFE/Woven Fiberglass Laminate
3M Dyneon™ CC603 PTFE, 15% Fiberglass Filled
GEHR Plastics PEEK-30GF Polyetheretherketone, 30% Glass Fiber
Hexcel® HexWeb® HRH-327 - 3/16 - 5.0 Fiberglass Reinforced Polyimide Honeycomb

PARLM9889 / 149042

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.