MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

CMW® ELKONITE 20SB tungsten, silver  (discontinued **)
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Refractory Metal; Tungsten Alloy

Material Notes: This material has been rebranded as a part of the NAECO® ELKON® product line.

ELKONITE® 20SB is made by a "press-sinter" method with a small addition of nickel used to activate the sintering. Because of fewer steps in manufacture this material is more economical than the Elkonite® 20S (press-sinter-infiltrate) counterpart. Size of Elkonite® 20SB contacts are limited due to warping. They can be made with a serrated back and excess silver to facilitate attachment. Elkonite® 20SB with its high refractory content is used in certain lower rated circuit breakers where their temperature rise is adequate. Some automotive circuit protectors use ELKONITE® 20SB operating against a silver alloy.

Information provided by CMW Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 14.9 g/cc0.538 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 100100
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000380 ohm-cm0.00000380 ohm-cm45 % IACS
 
Component Elements PropertiesMetricEnglishComments
Silver, Ag 27 %27 %
Tungsten, W 73 %73 %

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CMW® ELKONITE 35SB tungsten, silver
CMW® ELKONITE® 20S Infiltrated Tungsten Silver Contact Material ASTM B531, Class A, infiltrated
CMW® ELKONITE® 35S Silver Tungsten contact material ASTM B631, Class B, infiltrated
CMW® ELKONIUM 46 Silver Alloy
NAECO® ELKON® G17 Molybdenum Silver contact material ASTM 662, Class A, infiltrated

NCMW082 / 15896

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.