MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Saint-Gobain COHRlastic® R10470 Medium General-Purpose Silicone Sponge Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Foam

Material Notes: Description: Flexible, compressible COHRlastic silicone closed cell sponge is designed for high-performance gasketing, thermal shielding, vibration mounts and press pads. It is available in six constructions. R10470, a general-purpose silicone sponge, can be used in most applications.
Specification Notes: Meets Specifications: AMS 3195, MIL-R-6130 Type II, Grade B&C, MIL-R-46089, Boeing BMS 1-23, Douglas DMS 1597. All data based on a 0.0625 inch test sample.(Other thicknesses available.)
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0170 lb/in³ASTM D3574
Water Absorption <= 5.0 %ASTM D1056
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 90.0 psiASTM D412
Elongation at Break 150 %ASTM D412
Compressive Strength 10.0 psi
@Temperature 23.0 °C
ASTM D1056
Compression Set 25 %ASTM D1056
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 145 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 180 µin/in-°F
@Temperature 20.0 - 177 °C
Specific Heat Capacity 0.300 BTU/lb-°F
Thermal Conductivity 0.750 BTU-in/hr-ft²-°F
 
Descriptive Properties
ColorOrange-Tan, Black, or Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
P & P Technology Silicone Sponge
Rogers Corporation Bisco™ BF-1000 Cellular Silicone Foam
Overview of materials for Silicone Foam
Saint-Gobain COHRlastic® F-12 Silicone Foam
Saint-Gobain COHRlastic® R10480 Soft Low Compression Set Silicone Sponge Rubber

PSTGQZ252 / 68766

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.