MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Solvay Aluminum Sulfate
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Aluminum Sulfate, Solution, technical grade is a clear, water white to slightly yellow-brown liquid. It complies with the standards of the American Water Works Association B403-98. It has been certified by the National Sanitation Foundation (NSF) for use in the treatment of drinking water at a maximum dosage of 150 mg/L (dry basis).

Formula: Al2(SO4)3 (In aqueous solution

Nomenclature: Aluminum Sulfate, Solution Liquid Alum

CAS: 10043-01-3

CAS Index: Sulfuric Acid, Aluminum Salt (3:2)

Available in: North America

Uses: Chemical: In leather tanning, fur dressing, and catalyst manufacturing; Pulp and Paper: In the manufacture of paper; Textiles: As a mordant in dyeing; and Water Treatment: The treatment of water and waste water in coagulation, flocculation and phosphorous removal

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc
@Temperature 60.0 °C
0.0480 lb/in³
@Temperature 140 °F
For 8.25% Al2O3 solution
pH 0.20 - 2.50.20 - 2.5acidic to basic, For 8.25% Al2O3 solution
 2.2 - 4.02.2 - 4.01% solution, acidic to basic, For 8.25% Al2O3 solution
Molecular Weight 342.2 g/mol342.2 g/mol
 
Thermal PropertiesMetricEnglishComments
Melting Point -15.5 °C4.10 °FFreezing Point
 
Descriptive Properties
Assay>26.9%As Aluminum Sulfate, Anhydrous Al2(SO4)3
 >8.0%As available Water Soluble Al2O3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Potassium Aluminum Silicate, KALSi3O8
Master Bond MB600SCN Aqueous Based Electrically Conductive Sodium Silicate Coating
Sand, Dry
Overview of materials for Epoxy, Cast, Metal Filled
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded

WRHOD293 / 137524

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.