MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
A. Schulman Premi-Glas® 1265 VE 1265-VE (Injection Compression Molded) Glass Reinforced Vinyl Ester TMC  (discontinued **)
Categories: Polymer; Thermoset; Composite SMC; Filled/Reinforced Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC; Vinyl Ester

Material Notes: Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications.

Key features and benefits:

  • Designed for Injection or Injection-Compression molding
  • Excellent resistance to automotive chemicals and fluids, and to salt spray
  • Replaces Cast Metals for reduced Noise, Vibration and Harshness, plus molded-in color
  • TMC compounding process preserves glass integrity for excellent strength vs. BMC
  • Excellent thermal properties and elevated temperature modulus retention
  • Mechanical data below are from injection-compression panels; see separate data sheet for compression molded properties as required per some specifications

Market: Composite PowerTrain

Information provided by Premix.

A. Schulman has acquired this former Premix product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.80 g/ccASTM D792
Water Absorption 0.10 %ISO 62
Linear Mold Shrinkage 0.00070 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 4500 psiISO 527
Tensile Modulus 1.70e+6 psitangent; ISO 527
Flexural Strength 13000 psiISO 178
Flexural Modulus 1.60e+6 psiTangent; ISO 178
Poissons Ratio 0.274ISO 527-1
Shear Modulus 4.59 GPaCalculated
Izod Impact, Unnotched 2.80 ft-lb/inASTM D4812
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.0 µin/in-°F
@Temperature 20.0 °C
Z-direction; ASTM D696
CTE, linear, Transverse to Flow 15.0 µin/in-°F
@Temperature 20.0 °C
XY-direction; ASTM D696
Specific Heat Capacity 0.360 BTU/lb-°FASTM D1269E
Thermal Conductivity 2.78 BTU-in/hr-ft²-°FASTM D177
Deflection Temperature at 1.8 MPa (264 psi) 520 °FISO 75
Glass Transition Temp, Tg 370 °FASTM D4065-01

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman BMC 845 Vinyl Ester Molding Compounds, 30% Glass-Filled
A. Schulman Premi-Glas® 1266 (Injection Compression Molded) Glass Reinforced TMC
Haysite 44500 Vinyl Ester SMC, 30% Glass Reinforced
Quantum Composites QC-8700 63% Glass Fiber Reinforced Vinyl Ester SMC
A. Schulman BMC 845 30% Glass Filled Vinyl Ester

PPREMI05 / 58132

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.