MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ExxonMobil LD 201.48 Extrusion Coating for Milk Carton Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Extrusion Grade

Material Notes: Product Description: LD 201.48 is an LDPE extrusion coating grade, designed to have excellent processability combined with heat sealability and adhesion. It offers – Excellent neck-in/draw down balance, resulting in low edge trim i.e. less waste and high processing line speed. – Good barrier to water vapor, e.g. for applications in portion packaging (sugar, salt)

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: No
Applications:
  • Coextrusion Coating
  • Extrusion Coating
  • Extrusion Lamination
  • Foams
  • Food packaging
  • Industrial Packaging
  • Liquid Packaging
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.921 g/ccExxonMobil Method
Melt Flow 4.2 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Neck In 3.80 cm328 ft/min (100 m/min), Constant output at 35 rpm; ExxonMobil Method
 4.10 cm164 ft/min (50 m/min), Constant output at 35 rpm; ExxonMobil Method
Drawdown 3.30 m/sConstant output at 35 rpm; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Melting Point 228 °FPeak Melting Temperature; ExxonMobil Method
Vicat Softening Point 95.0 °CASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Superwool® VF Shapes and Boards Plus Carton Thermal Ceramic
ATI Allvac® Nickelvac® H-X Nickel Superalloy, Heat Treatment: 1177°C (2150°F) Anneal
Braskem BI 818 LDPE Injection Molding Polyethylene
Chevron Phillips 4538B LDPE Injection Molding Resin
Chevron Phillips KN 230B LDPE Injection Molding Resin

PEXB049 / 37354

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.