MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Röhm PLEXIGLAS® GS (0F00) Acrylic Rods and Tubes  (discontinued **)
Categories: Polymer; Thermoplastic; Acrylic (PMMA)

Material Notes: Product PLEXIGLAS® XT rods and tubes are the clearest extruded tubes on the market today delivering brilliant quality, superior performance, and durability. PLEXIGLAS® XT rods and tubes are characterized by their flawless optics, and perfectly smooth surface free of striations. White or frosted satin surface finishes provide excellent diffused light creating a velvety nonglare surface. High-quality, design-orientated applications within the architectural lighting industry can be easily created. (for information see PLEXIGLAS® Satinice.). Create impressive lighting effects by end lighting our PLEXIGLAS® LED (EndLighten T) rods. Colored extruded PLEXIGLAS® XT rods and tubes are also available and if additional impact strength is required they can be produced with our acrylic impact modified polymer. You will find more detailed information in the Sales Handbook. PLEXIGLAS® GS tubes are produced in the cast rotation process. Cast rods and square rods are made of casted semi-finished products. All cast forms have polished surfaces.

Features & Benefits

  • Excellent light transmission and brilliance
  • Outstanding weather resistance
  • Easy to fabricate
  • High surface hardness
  • Light weight – half of the weight of glass
  • 100% recyclable
  • 11 times more break resistant than glass
PLEXIGLAS® XT rods and tubes exhibit the following features:
  • Excellent surface appearance
  • Tight tolerances
  • Conformity to food grade specifications (only applies to colorless)
  • UV-transmitting
Cast rods and tubes have:
  • Polished finish
  • Higher molecular weight which results in a more solvent resistant product.
Applications: Due to the above characteristics PLEXIGLAS® rods and tubes are ideally suitable for.
  • Architectural interior & exterior lighting
  • Contemporary furniture.
  • Luxury brand merchandizing, store fixtures, P.O.P. & trade show displays
  • Industrial pneumatic delivery and conveying systems
  • Decorative architectural features

The former Evonik Methacrylates business has been sold to Röhm GmbH (Roehm).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPa
@Temperature 70.0 °C
ISO 527-2/1B/5
 80.0 MPa
@Temperature 23.0 °C
ISO 527-2/1B/5
 110 MPa
@Temperature -40.0 °C
ISO 527-2/1B/5
Modulus of Elasticity 3.30 GPashort-time value
Izod Impact, Notched (ISO) 1.60 kJ/m²ISO 180/1A
Charpy Impact Unnotched 15.0 kJ/m²ISO 179/1 fu
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 µin/in-°F
@Temperature 0.000 - 50.0 °C
DIN 53752-A
Maximum Service Temperature, Air 80.0 °C
Vicat Softening Point 115 °CB50; ISO 306
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 92 %DIN 5036

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Röhm Plexiglas® GS 0Z09 (209) Cast Acrylic
Röhm Plexiglas® GS 0F00 (222) Cast Acrylic
Röhm Plexiglas® GS 0F00 (233) Cast Acrylic
Chi Mei Acryrex® CM-205 PMMA
Lendell Parapet HH-1000L PMMA, Heat Resistant

PEVONIL014 / 196220

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.