MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Atom Adhesives AA-BOND FDA2 Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: AA-BOND FDA2 is a medium viscosity epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and received Class VI approval. AA-BOND FDA2 is two part amber adhesive used and cured at room temperature for bonding, laminating and repair applications by manufacturers of food preparation, processing and packaging equipment and devices. AA-BOND FDA2 provides low permeability to gases and vapors, and good resistance to water, weather, petroleum solvents, lubricants, to mild acids and alkalis, and to many other organic and inorganic compounds.

Appearance: Amber

Cure Type: Heat cure or Room Temperature

Benefits:

  • Medium viscosity
  • Class VI approved
  • Low permeability
  • Good resistance
  • Easily mixed
Mix Ratio by weight: 100:100/Resin:Hardener

Substrates: Most metals, ceramic, glass and plastics.

Typical Application: Bonding, laminating and repair applications by manufacturers of food preparation, processing and packaging equipment, and by manufacturers of catheters, hearing aids, dental products and other biomedical instruments and devices.

Information provided by Atom Adhesives

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccuncured
Solids Content 100 %100 %reactive, uncured
Viscosity 12000 - 16000 cP12000 - 16000 cPuncured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7979
Elongation at Yield 9.0 %9.0 %cured
Adhesive Bond Strength 12.4 MPa1800 psiLap shear, alum to alum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.20e+14 ohm-cm1.20e+14 ohm-cm
Dielectric Constant 3.4
@Frequency 1000 Hz
3.4
@Frequency 1000 Hz
Dielectric Strength 16.5 kV/mm420 kV/in
Dissipation Factor 0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 52.9 µm/m-°C29.4 µin/in-°F
Maximum Service Temperature, Air 145 °C293 °F
Minimum Service Temperature, Air -70.0 °C-94.0 °F
Glass Transition Temp, Tg 54.0 °C129 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 240 min
@Temperature 65.0 °C
1.00 - 4.00 hour
@Temperature 149 °F
 1440 min
@Temperature 25.0 °C
24.0 hour
@Temperature 77.0 °F
Pot Life 45.0 min45.0 minuncured
 
Compliance PropertiesMetricEnglishComments
USP Class VI YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PATOM027 / 172342

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.