MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ExxonMobil 10W Mobil Hydraulic
Categories: Fluid; Lubricant

Material Notes: Mobil Hydraulic 10W is a high performance hydraulic oil formulated from advanced base oils and a balanced additive system designed to satisfy a wide range of heavy-duty hydraulic equipment requirements. This product is specifically engineered using an effective balance of ashless dispersants and metallic detergents combined with inhibitors to control oxidation, wear, corrosion and rust. Mobil Hydraulic 10W is used in a wide range of on and off-highway hydraulic applications.

Hydraulic systems and components used in conjunction with equipment from American, European, and Japanese manufacturers; Hydraulic systems where wide ambient temperatures are encountered; Hydraulic systems containing gears and bearings where good anti-wear properties are required; On and off-highway industries including: trucking, construction, mining, quarrying, and agriculture

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.877 g/cc
@Temperature 15.0 °C
ASTM D4052
Viscosity Measurement 107Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 37.7 cStASTM D445
Kinematic Viscosity at 100°C (212°F) 6.1 cStASTM D445
Ash 0.50 %Sulfated Ash, wt%; ASTM D874
 
Chemical PropertiesOriginal ValueComments
Total Base Number 4.0mg KOH/g; ASTM D2896
 
Thermal PropertiesOriginal ValueComments
Pour Point -30.0 °CASTM D97
Flash Point 232 °CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Phillips 66 MV22 Super Hydraulic Oil
Phillips 66 FR Hydraulic Fluid ISO Grade 100
ConocoPhillips Hydroclear® AW 46 Hydraulic Fluid
ChevronTexaco ECO® ISO 46 Hydraulic Oil AW
Unipetrol R2 Heavy Fuel Oil

WEXXON063 / 75488

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.