MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Teijin Films Melinex® ST328 Polyester Film, 1400 Gauge
Categories: Polymer; Film; Thermoplastic; Polyester, TP; Polyester Film

Material Notes: Melinex® ST328 is an exceptionally white, opaque film with a satin finish. It is pretreated on both surfaces to promote adhesion to a wide range of solvent-based and UV-curable graphics inks and varnishes, silver conducting inks and dielectrics, and has been heat stabilized to give excellent dimensional stability at temperatures up to 302°F.

Typical Applications: Melinex® ST328 has been developed for use in screen-printed medical test strips where a white background appearance is required. The tight thickness control of this film ensures reliable insertion into reading devices.

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccASTM D1505-85
Brightness 85.0 %Whiteness; ASTM E313-79
Thickness 14.0 mil
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction, Dynamic 0.40A-B; ASTM D1894
Film Tensile Strength at Break, MD 22000 psiASTM D882A
Film Tensile Strength at Break, TD 24000 psiASTM D882A
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.0 µm/m-°C
@Temperature 20.0 - 50.0 °C
Melting Point 491 - 500 °FASTM E794-85
Shrinkage, MD <= 0.20 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
Shrinkage, TD <= 0.10 %
@Temperature 150 °C,
Time 1800 sec
Unrestrained
 
Optical PropertiesOriginal ValueComments
Gloss 45 %60°; ASTM D1003
Yellow Index -1.50 %ASTM D1925
Transmission, Visible 1.1 %TLT; ASTM D1003
 
Descriptive Properties
Color-0.1a
 -0.8b
 96.8L

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Teijin Films Melinex® FRP Polyester Film, 92 Gauge
DuPont Teijin Films Melinex® D316 Polyester Film, 200 Gauge
DuPont Teijin Films Melinex® CORE 2 Polyester Film
DuPont Teijin Films Melinex® HS2 Polyester Film
DuPont Teijin Films Melinex® RFL1 Polyester Film, 600 Gauge

PDTZ9229 / 139557

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.